Galvanic Corrosion with Electrode Deformation

Application ID: 12423


This 2D model demonstrates how to model a galvanic couple in which the corrosion of the anode causes a geometry deformation. The parameter data used is for an Magnesium Alloy (AE44) - mild steel couple in brine solution (salt water).


This model example illustrates applications of this type that would nominally be built using the following products: